This study presents definition of the types of lightweight concrete and some studies, which use the volcanic scoria aggregates to produce structural lightweight concrete. Several concrete mixes were designed, and different tests were performed to determine its properties.


Artificial intelligence review:
Research summary
تقدم هذه الدراسة تعريفًا بأنواع الخرسانة الخفيفة وبعض الدراسات التي استخدمت الحصويات البركانية (السكوريا) في إنتاجها. تضمنت الدراسة توصيفًا لهذه الحصويات وتصميم عدة خلطات خرسانية تختلف بعيار الاسمنت المستخدم. تم إجراء مجموعة من الاختبارات على عينات مكعبية وأسطوانية مأخوذة من هذه الخلطات لتعيين خصائص الخرسانة الناتجة، مثل الكثافة والمقاومة على الضغط والشد بالانفلاق ومعامل المرونة ومخطط علاقة (إجهاد-تشوه) في حالة الضغط. أظهرت النتائج إمكانية استخدام حصويات السكوريا لإنتاج خرسانة خفيفة تحقق متطلبات الخرسانة الخفيفة الإنشائية حسب الكود الأمريكي ACI 213R-03. كما بينت الدراسة أن الحد الأعلى لمقاومة الخرسانة الخفيفة على الضغط يعتمد على مقاومة الحصويات الخفيفة أكثر من زيادة عيار الاسمنت، وأن شكل مخطط علاقة (إجهاد-تشوه) مشابه لحالة الخرسانة العادية مع زيادة لقيمة التشوه الموافق لقيمة الإجهاد الأعظمي.
Critical review
دراسة نقدية: تعتبر هذه الدراسة خطوة هامة في مجال استخدام الحصويات البركانية لإنتاج الخرسانة الخفيفة، إلا أن هناك بعض النقاط التي يمكن تحسينها. أولاً، كان من الممكن توسيع نطاق العينات المدروسة لتشمل أنواعًا أخرى من الحصويات الخفيفة المتوفرة محليًا. ثانيًا، لم تتناول الدراسة بشكل كافٍ تأثير الظروف البيئية المختلفة على أداء الخرسانة الخفيفة المنتجة. ثالثًا، كان من الممكن إجراء مقارنة أكثر تفصيلًا بين الخرسانة الخفيفة المنتجة باستخدام السكوريا والخرسانة العادية من حيث التكلفة والفعالية الإنشائية. وأخيرًا، يوصى بإجراء دراسات مستقبلية لمعرفة ديمومة هذه الخرسانة وجدواها الاقتصادية بشكل أكثر تفصيلًا.
Questions related to the research
  1. ما هي الخصائص التي تم دراستها في هذه البحث للخرسانة الخفيفة؟

    تم دراسة الكثافة، والمقاومة على الضغط، والشد بالانفلاق، ومعامل المرونة، ومخطط علاقة (إجهاد-تشوه) في حالة الضغط.

  2. ما هو الحد الأعلى لمقاومة الخرسانة الخفيفة على الضغط وفقًا للدراسة؟

    الحد الأعلى لمقاومة الخرسانة الخفيفة على الضغط يعتمد على مقاومة الحصويات الخفيفة أكثر من زيادة عيار الاسمنت.

  3. ما هو تأثير زيادة عيار الاسمنت على مقاومة الخرسانة الخفيفة؟

    زيادة عيار الاسمنت تسبب زيادة للمقاومة على الضغط بشكل واضح حتى حد معين تصبح عنده مقاومة الخرسانة معتمدة على مقاومة الحصويات ونوعها أكثر من اعتمادها على مقاومة الرابط الاسمنتي.

  4. ما هي التوصيات المستقبلية التي قدمتها الدراسة؟

    يوصى بإجراء دراسة لمعرفة ديمومة هذه الخرسانة وجدواها الاقتصادية، بالإضافة إلى دراسة تأثير الظروف البيئية المختلفة على أدائها.


References used
ACI Committee 213R-03, 2003- Guide for Structural Lightweight Aggregate Concrete. American Concrete Institute, 38p
ASTM C330-99, 1999 -Standard Specification for Lightweight Aggregates for Structural Concrete. 6p
Slaby, A; Aziz, K; Hadeed, A. 2008 -Mechanical Properties of Porcelinite Reinforced Concrete Beams. IJCE, Vol. 10, 25P
rate research

Read More

Compacting hot mixes asphalt (HMA) at low temperatures or mixing it in the asphalt at high temperatures is a constant source of concern to researchers, as compacting and mixing at non-ideal temperatures leads to adverse results, which negatively affect the properties of asphalt concrete and lead to problems paving.
Concrete considers as the most popular building material because of the many advantages that it has. This come up with a huge amount of concrete waste. As a way to produce a concrete which is friend to environment, four percentages 0%, 50%, 75%, 100% of coarse recycled aggregate as replacement of natural coarse aggregate in concrete mix are used in this research. The work ability and wet and dry density are presented in this study. The compressive strength at age of 7, 28, 56 days are estimated, also splitting tensile strength and modulus of elasticity are founded at 28 day. The study shows that when The percentage of recycled aggregate exceeds 50% in concrete mix the mechanical properties reduce. When 100% of recycled aggregate is used the compressive strength, splitting tensile strength and elastic modulus decrease by 14%, 22%, 25% respectively, so it is possible to use recycled aggregate concrete in production of non-structural elements.
The physical properties of gravel play an important role on the quality of concrete industry in local workshops. Because they constitute a main role in various concrete mix design. It's necessary to understand the importance of the physical proper ties of gravel and It's improving role in the concrete mixes. This research aimed to study the role of the properties of gravel on the concrete mixes manufacture.
Ultra-High-performance concrete (UHPC) attracted attention in the civil engineering industry in recent times, because it has high resistance and rigidity . What provided the UHPC of skinny clips justifies using it in high buildings to take advanta ge of pressure and tensile its resistance . The largest use of this material in the bridges because of its high resistance which suitable for large loads as well as a valid treated outside the center and sustainability of the high buildings, We study several models of building and we use this material in several elements of these . We found after analysis of the high efficiency of this models, especially in Diaframat.
This paper studies a practical laboratory research of the possibility of utilizing the natural resources available in the country, namely Basalt, which is available in large quantities in the southern region (Al-Suwayda) in order to demonstrate the extent to which it meets the requirements of standard specifications for use in the manufacture of (Reinforced) concrete by means of testing the resistance of pressure and tensile by splitting and the elasticity coefficient of hardened (rigid concrete) at Different ages (3-7- 28) days. As a result, pressure resistance tests increased by approximately 20 % with the maturating period progress of concrete mixtures. The pressure resistance of concrete mixtures prepared using basalt pebbles was approximately 18% higher than the pressure resistance of concrete formed usingcalcite(calcareous) pebbles in ages above 7 days There was also a slight decrease of 8% in the split tensile resistance of the studied samples prepared with basalt minerals , compared with the samples prepared using calcite (calcareous) pebble and this resistance increases over time . As for the elasticity coefficient , a 20% increase in the elasticity coefficient of the concrete was noticed with the maturating of the concrete mixtures compared to the referential mixture.
comments
Fetching comments Fetching comments
Sign in to be able to follow your search criteria
mircosoft-partner

هل ترغب بارسال اشعارات عن اخر التحديثات في شمرا-اكاديميا