The objective of this research is to study the effect of wood ash in rheological properties of Self – compacting mortar (SCM). By implemented some mixtures with different percentage from wood ash with two kinds of cement and three kinds of super plasticizer and study the effect in slump flow and yield stress to this mixtures.


Artificial intelligence review:
Research summary
تتناول هذه الدراسة تأثير إضافة رماد الخشب على الخواص الريولوجية للمونة ذاتية التوضع (SCM). تعتبر المونة ذاتية التوضع قاعدة لمعرفة قابلية تشغيل البيتون ذاتي التوضع (SCC)، وتقييم خصائصها جزء متمم في تصميم خلطة البيتون ذاتي التوضع. يهدف البحث إلى دراسة تأثير رماد الخشب على الخواص الريولوجية للمونة من خلال تشكيل عدة خلطات بنسب مختلفة من الرماد ومع نوعين مختلفين من الاسمنت وباستخدام ثلاثة أنواع من الملدنات. أظهرت النتائج أن زيادة نسبة رماد الخشب تؤدي إلى انخفاض قيمة قطر الانتشار والانتشار النسبي، بينما تتزايد قيمة إجهاد الخضوع مع زيادة نسبة رماد الخشب. تم استخدام نوعين من الاسمنت (اسمنت طرطوس واسمنت السبع) وثلاثة أنواع من الملدنات، وأظهرت النتائج أن فعالية الملدنات تختلف باختلاف نوع الاسمنت المستخدم. توصي الدراسة بإجراء مزيد من الأبحاث على تأثير رماد الخشب على المقاومة الميكانيكية للمونة المكافئة ومع أنواع الملدنات المختلفة وأصناف الاسمنت المختلفة.
Critical review
دراسة نقدية: تعتبر هذه الدراسة خطوة مهمة في مجال تحسين خواص المونة ذاتية التوضع باستخدام مواد بديلة مثل رماد الخشب. ومع ذلك، يمكن توجيه بعض النقد البناء للدراسة. أولاً، لم يتم التطرق بشكل كافٍ إلى الآثار البيئية لاستخدام رماد الخشب وكيفية التخلص منه بعد انتهاء عمر الخدمة للبيتون. ثانياً، كان من الأفضل تضمين تحليل اقتصادي يوضح الفوائد المالية لاستخدام رماد الخشب مقارنة بالإضافات التقليدية. ثالثاً، الدراسة تركزت بشكل كبير على الخواص الريولوجية دون التطرق بشكل موسع إلى الخواص الميكانيكية الأخرى مثل مقاومة الضغط والشد. وأخيراً، كان من الممكن تحسين الدراسة بتوسيع نطاق التجارب لتشمل أنواع أخرى من الاسمنت والملدنات لتقديم نتائج أكثر شمولية.
Questions related to the research
  1. ما هو الهدف الرئيسي من هذه الدراسة؟

    الهدف الرئيسي من الدراسة هو دراسة تأثير رماد الخشب على الخواص الريولوجية للمونة ذاتية التوضع (SCM) من خلال تشكيل عدة خلطات بنسب مختلفة من الرماد ومع نوعين مختلفين من الاسمنت وباستخدام ثلاثة أنواع من الملدنات.

  2. ما هي النتائج الرئيسية التي توصلت إليها الدراسة؟

    أظهرت النتائج أن زيادة نسبة رماد الخشب تؤدي إلى انخفاض قيمة قطر الانتشار والانتشار النسبي، بينما تتزايد قيمة إجهاد الخضوع مع زيادة نسبة رماد الخشب.

  3. ما هي التوصيات التي قدمتها الدراسة؟

    توصي الدراسة بإجراء مزيد من الأبحاث على تأثير رماد الخشب على المقاومة الميكانيكية للمونة المكافئة ومع أنواع الملدنات المختلفة وأصناف الاسمنت المختلفة، بالإضافة إلى دراسة تأثير إضافة رماد الخشب مع أنواع البيتون المختلفة لتخليص البيئة من آثاره السلبية.

  4. ما هي أنواع الاسمنت والملدنات المستخدمة في الدراسة؟

    تم استخدام نوعين من الاسمنت (اسمنت طرطوس واسمنت السبع) وثلاثة أنواع من الملدنات في الدراسة.


References used
M. Sahmaran, H. A. Christianto, Ismail O. Yaman. The effect of chemical admixtures and mineral additives on the properties of self-compacting mortars,2005 Ankara, Turkey
Cheah Chee Ban , Mahyuddin RamliThe implementation of wood waste ash as a partial cement replacement material in the production of structural grade concrete and mortar, Universiti Sains Malaysia,2011
M. Abdullahi , Characteristics of Wood ASH/OPC Concrete , Civil Engineering Department, Federal University of Technology, P.M.B. 65, Minna, Niger 2006
rate research

Read More

Asphalt plays the role of envelope and bonding in asphalt gable, and is exposed to a range of changes that start from the stage of production of asphalt mosses to the stage of investment under the influence of traffic loads and weather factors. The aim of this research is to investigate the possibility of using polypropylene polymer to modify the properties of the asphalt binder and to increase its resistance to high temperatures and different climatic conditions by modifying the asphalt by adding polypropylene by (1, 2, 3, 4, 6, 8%) And perform traditional tests on modified asphalt samples . Using Thin film oven test RTFOT test to perform the short-term Aging on normal and modified asphalt samples, heat loss, residual Penetration and aging index, And conduct a structural composition test to determine asphalt compounds. The results of the study showed that the values of Penetration tend to decrease with the increase of the percentage of addition while the degree of Softening point. The results showed increased resistance of asphalt modified to the thermal conditions. The optimum percentage of polypropylene is 3% Loss on heat at the lowest level.
It was investigated in this study the influence of Carboxymethylcellolose (CMC) solution concentration, temperature, and pH on the rheological properties according to the shear stress as function of shear rate. Experimental results show that shea r stress increase at all operational conditions as the shear rate increase. When the shear rate is constant, the shear stress increases also with the increasing of both concentration and pH as well as the decreasing of temperature.
The results showed the possibility of getting at a wide rang of board with different properties, and all investigated percentage had special properties which to use in industrial application, also the result showed the possibility to produce these bo ard without pretreatment of particles wood or without addition any virgin plastic to RLDPE The results showed the possibility of getting of a wide spectrum of boards with different properties, and all studied percentages had special properties which allow them to use in industrial application, also the result showed the possibility to produce these boards without treatment of the wood particles or without addition any virgin plastic to RLDPE
The ideal selection of raw materials in manufacturing process is a very important step to develop this process and to improve the product. For this purpose, we search for initial parameters to guide us in using clay materials (wherever it locate) i n ceramic industry. These parameters depend on physical properties of clay (Atterberg Limits). We follow experimental and analytical methods for laboratories tests applied or clay, and for ceramic samples tests. We deduct initial parameters which determine technical specification values for ceramic product, and we derived mathematical formulas between clay properties and technical specification for ceramic product. These parameters and formulas help us to achieve ideal investment for clay ambushes either as pure raw materials or with suitable additives to reach on acceptable value for water absorption of ceramic product which, at the end, specify the type of product according to international specification.
This research study the impact of additions to improve limestone mortar properties to become comparable to hydraulic lime which is used in other countries, by using additions relative to that were used in the old mortar, also used modern additions like fiber glass to limit unwanted contraction in the use of limestone mortar, , especially in arid environments.
comments
Fetching comments Fetching comments
Sign in to be able to follow your search criteria
mircosoft-partner

هل ترغب بارسال اشعارات عن اخر التحديثات في شمرا-اكاديميا