إن الحصول على التطابق اللوني النهائي مع الأسنان الطبيعية عند الترميم بالخزف الكامل الزجاجي صعب التحقيق في أغلب الأحيان، و لكنه مهم جداً لنجاح هذا النوع من الترميمات تجميلياً. هدف هذا البحث إلى تقييم تأثير لون إسمنت الإلصاق في اللون النهائي للتاج المصنوع من الخزف الكامل الزجاجي لنظام IPS e.max.
Usually, it's hard to reach the final color identity with normal teeth when using
full glass ceramic, but this matter is very important for the cosmetic successful of these restorations. This
in vitro study evaluated the effect of cement color on the final color of full crown glass ceramic of system
IPS e.max.
References used
Joiner A. Tooth Color: A review of The Literature. J Dent 2004; 32: 3-12
Nagai S, Yoshida A, Sakai M, Kristiansen J. Clinical evaluation of perceptibility of color differences between natural teeth and all-ceramic crowns, Elsevier Ltd, United States, 2009, p58
O'Brien WJ. Dental Materials and Their Selection, 3rd Ed., Quintessence Publishing, Michigan, 2002, p58
Porcelain has a long history of fixed prosthodontics to achieve optimum beauty by color. However, there is a lack of information on how the color of different thicknesses of ivory porcelain is affected by repeated exposure to baking.
Objective: is to study the effect of colored (non-opaque) adhesive resin cement and opaque adhesive resin cement on color matching of full ceramic crowns set on severe discolored abutments.
Materials and Methods: Sample consisted of 15 full cerami
This study aims to recognize the effect of Variolink Veneer (V.V) cement colors used in luting thin veneers fabricated from (IPS e-max) porcelain on the final resulting color. A sample of (30) thin veneers in (A1-A2-A3-A3,5( colors is used. The venee
Color stability is an important factor to ensure the long-term of esthetic success
of ceramic restoration, there are several factors affect color stability, such as repeated firing.
Aim of Study: Color Difference comparison between two types of cer
An appropriate bond between glass‑ionomer and the superficial
resin materials is very important for the success of sandwich
technique. The aim of the present in vitro study was to evaluate the
effect of three surface treatments of conventional glass‑ionomer on
its shear bond strength to giomer