In terms of mixing graded TiO2 and SnO2 powders by solid-state reaction method, ITO was prepared. Using electron beam gun technology, ITO films with different thicknesses were prepared. The influence of film thickness on structure, electrical and optical properties was studied. The XRD patterns were utilized to determine the structural parameters (lattice strain and crystallite size) of ITO with different thicknesses. It is observed that the average crystallite size increases as the film thickness increases, but the lattice strain decreases. SEM shows that as the film thickness increases, the grain size of ITO increases and improves. The electrical properties of ITO films with different thicknesses were measured by the standard four-point probe method. It can be seen that as the thickness of the ITO film increases from 75 nm to 325 nm, the resistivity decreases from 29x10^-4 Ohm/cm to 1.65x10^-4 Ohm/cm. This means that ITO films with lower electrical properties will be more suitable for high-efficiency CdTe solar cells. Three optical layer models (adhesive layer of the substrate/B-spline layer of ITO film/surface roughness layer) are used to calculate the film thickness with high-precision ellipsometry. In the higher T(lambda) and R(lambda) absorption regions, the absorption coefficient is determined to calculate the optical energy gap, which increases from 3.56 eV to 3.69 eV. Finally, the effects of ITO layers of various thicknesses on the performance of CdS/CdTe solar cells are also studied. When the thickness of the ITO window layer is 325 nm, Voc = 0.82 V, Jsc = 17 mA/cm2, and FF = 57.4%, the highest power conversion efficiency (PCE) is 8.6%.



قيم البحث

اقرأ أيضاً

This work reports on the synthesis of CrO2 thin films by atmospheric pressure CVD using chromium trioxide (CrO3) and oxygen. Highly oriented (100) CrO2 films containing highly oriented (0001) Cr2O3 were grown onto Al2O3(0001) substrates. Films displa y a sharp magnetic transition at 375 K and a saturation magnetization of 1.92 Bohr magnetons per f.u., close to the bulk value of 2 Bohr magnetons per f.u. for the CrO2. Keywords: Chromium dioxide (CrO2), Atmospheric pressure CVD, Spintronics.
Photoelectric conversion efficiency of organic-inorganic perovskite solar cells has been rapidly raised and attracted great attention in recent years. The quality of perovskite films is vital for the performance of devices. We used the anti-solvent m ethod to prepare CH$_3$NH$_3$PbI$_3$ thin films by spin coating and dried them at various temperature to transform adduct MAI.PbI$_2$.DMSO into CH$_3$NH$_3$PbI$_3$. We researched in detail on the relationship between surface morphology of MAPbI$_3$ thin films fabricated by the anti-solvent method and various drying temperature. We found that surface roughness and grain size of CH$_3$NH$_3$PbI$_3$ films together increased with increasing drying temperature. The larger grain size could efficiently reduce crystal boundaries which is advantageous for the suppression of photo-induced charge carrier recombination resulting in increase of FF. However, increase of surface roughness resulted in larger contact area at interface which might produce more tarp states and poorer wettability of HTM solution leading in decrease of Jsc. Surface morphology of MAPbI3 layer on the performance of solar cell devices is also an important research issue. By optimizing the drying temperature to 60 oC, the highest efficiency of 14.4% was achieved for the CH3NH3PbI3-based solar cell devices.
91 - E. Colombo , A. Bosio , S. Calusi 2016
This paper reports on the investigation of the electronic properties of a thin film CdS/CdTe solar cell with the Ion Beam Induced Charge (IBIC) technique. The device under test is a thin film (total thickness around 10 um) multilayer heterojunction s olar cell, displaying an efficiency of 14% under AM1.5 illumination conditions. The IBIC measurements were carried out using focused 3.150 MeV He ions raster scanned onto the surface of the back electrode. The charge collection efficiency (CCE) maps show inhomogeneous response of the cell to be attributed to the polycrystalline nature of the CdTe bulk material. Finally, the evolution of the IBIC signal vs. the ion fluence was studied in order to evaluate the radiation hardness of the CdS/CdTe solar cells in view of their use in solar modules for space applications.
Epitaxial NbO2 (110) films, 20 nm thick, were grown by pulsed laser deposition on Al2O3 (0001) substrates. The Ar/O2 total pressure during growth was varied to demonstrate the gradual transformation between NbO2 and Nb2O5 phases, which was verified u sing x-ray diffraction, x-ray photoelectron spectroscopy, and optical absorption measurements. Electric resistance threshold switching characteristics were studied in a lateral geometry using interdigitated Pt top electrodes in order to preserve the epitaxial crystalline quality of the films. Volatile and reversible transitions between high and low resistance states were observed in epitaxial NbO2 films, while irreversible transitions were found in case of Nb2O5 phase. Electric field pulsed current measurements confirmed thermally-induced threshold switching.
An optoelectronic optimization was carried out for an AlGaAs solar cell containing (i) an n-AlGaAs absorber layer with a graded bandgap and (ii) a periodically corrugated Ag backreflector combined with localized ohmic Pd-Ge-Au backcontacts. The bandg ap of the absorber layer was varied either sinusoidally or linearly. An efficiency of 33.1% with the 2000-nm-thick n-AlGaAs absorber layer is predicted with linearly graded bandgap along with silver backreflector and localized ohmic backcontacts, in comparison to 27.4% efficiency obtained with homogeneous bandgap and a continuous ohmic backcontact. Sinusoidal grading of the bandgap {is predicted to enhance} the maximum efficiency to 34.5%. Thus, grading the bandgap of the absorber layer, along with a periodically corrugated Ag backreflector and localized ohmic Pd-Ge-Au backcontacts can help realize ultrathin and high-efficient AlGaAs solar cells for terrestrial applications.
التعليقات
جاري جلب التعليقات جاري جلب التعليقات
سجل دخول لتتمكن من متابعة معايير البحث التي قمت باختيارها
mircosoft-partner

هل ترغب بارسال اشعارات عن اخر التحديثات في شمرا-اكاديميا