Glass films created by vapor-depositing molecules onto a substrate can exhibit properties similar to those of ordinary glasses aged for thousands of years. It is believed that enhanced surface mobility is the mechanism that allows vapor deposition to create such exceptional glasses, but it is unclear how this effect is related to the final state of the film. Here we use molecular dynamics simulations to model vapor deposition and an efficient Monte Carlo algorithm to determine the deposition rate needed to create ultra-stable glassy films. We obtain a scaling relation that quantitatively captures the efficiency gain of vapor deposition over bulk annealing, and demonstrates that surface relaxation plays the same role in the formation of vapor-deposited glasses as bulk relaxation does in ordinary glass formation.

قيم البحث

اقرأ أيضاً

Glasses are nonequilibrium solids with properties highly dependent on their method of preparation. In vapor-deposited molecular glasses, structural organization could be readily tuned with deposition rate and substrate temperature. Herein, we show th e atomic arrangement of strong network forming GeO2 glass is modified at medium range (< 2 nm) through vapor deposition at elevated temperatures. Raman spectral signatures distinctively show the population of 6-membered GeO4 rings increases at elevated substrate temperatures. Deposition near the glass transition temperature is more efficient than post-growth annealing in modifying atomic structure at medium range. The enhanced medium range organization correlates with reduction of the room temperature internal friction. Identifying the microscopic origin of room temperature internal friction in amorphous oxides is paramount to design the next generation interference coatings for mirrors of the end test masses of gravitational wave interferometers, in which the room temperature internal friction is a main source of noise limiting their sensitivity.
In-situ NMR spin-lattice relaxation measurements were performed on several vapor deposited ices. The measurements, which span more than 6 orders of magnitude in relaxation times, show a complex spin-lattice relaxation pattern that is strongly depende nt on the growth conditions of the sample. The relaxation patterns change from multi-timescale relaxation for samples grown at temperatures below the amorphous-crystalline transition temperature to single exponential recovery for samples grown above the transition temperature. The slow-relaxation contribution seen in cold-grown samples exhibits a temperature dependence, and becomes even slower after the sample is annealed at 200K. The fast-relaxation contribution seen in these samples, does not seem to change or disappear even when heating to temperatures where the sample is evaporated. The possibility that the fast relaxation component is linked to the microporous structures in amorphous ice samples is further examined using an environmental electron scanning microscope. The images reveal complex meso-scale microporous structures which maintain their morphology up to their desorption temperatures. These findings, support the possibility that water molecules at pore surfaces might be responsible for the fast-relaxation contribution. Furthermore, the results of this study indicate that the pore-collapse dynamics observed in the past in amorphous ices using other experimental techniques, might be effectively inhibited in samples which are grown by relatively fast vapor deposition.
The atomic theory of elasticity of amorphous solids, based on the nonaffine response formalism, is extended into the nonlinear stress-strain regime by coupling with the underlying irreversible many-body dynamics. The latter is implemented in compact analytical form using a qualitative method for the many-body Smoluchowski equation. The resulting nonlinear stress-strain (constitutive) relation is very simple, with few fitting parameters, yet contains all the microscopic physics. The theory is successfully tested against experimental data on metallic glasses, and it is able to reproduce the ubiquitous feature of stress-strain overshoot upon varying temperature and shear rate. A clear atomic-level interpretation is provided for the stress overshoot, in terms of the competition between the elastic instability caused by nonaffine deformation of the glassy cage and the stress buildup due to viscous dissipation.
Integration of graphene with Si microelectronics is very appealing by offering potentially a broad range of new functionalities. New materials to be integrated with Si platform must conform to stringent purity standards. Here, we investigate graphene layers grown on copper foils by chemical vapor deposition and transferred to silicon wafers by wet etch and electrochemical delamination methods with respect to residual sub-monolayer metallic contaminations. Regardless of the transfer method and associated cleaning scheme, time-of-flight secondary ion mass spectrometry and total reflection x-ray fluorescence measurements indicate that the graphene sheets are contaminated with residual metals (copper, iron) with a concentration exceeding 10$^{13}$ atoms/cm$^{2}$. These metal impurities appear to be partly mobile upon thermal treatment as shown by depth profiling and reduction of the minority charge carrier diffusion length in the silicon substrate. As residual metallic impurities can significantly alter electronic and electrochemical properties of graphene and can severely impede the process of integration with silicon microelectronics these results reveal that further progress in synthesis, handling, and cleaning of graphene is required on the way to its advanced electronic and optoelectronic applications.
Nanodiamond crystals containing single color centers have been grown by chemical vapor deposition (CVD). The fluorescence from individual crystallites was directly correlated with crystallite size using a combined atomic force and scanning confocal f luorescence microscope. Under the conditions employed, the optimal size for single optically active nitrogen-vacancy (NV) center incorporation was measured to be 60 to 70 nm. The findings highlight a strong dependence of NV incorporation on crystal size, particularly with crystals less than 50 nm in size.