ترغب بنشر مسار تعليمي؟ اضغط هنا

83 - S. White 2014
In polarized proton operation in the Relativistic Heavy Ion Collider (RHIC) coherent beam-beam modes are routinely observed with beam transfer function measurements. These modes can become unstable under external excitation or in the presence of impe dance. This becomes even more relevant in the presence of head-on compensation, which reduces the beam-beam tune spread and hence Landau damping. We report on experiments and simulations carried out to understand the impact of coherent modes on operation with electron lenses.
Heavy ion cross sections totaling several hundred barns have been calculated previously for the Relativistic Heavy Ion Collider (RHIC) and the Large Hadron Collider (LHC). These total cross sections are more than an order of magnitude larger than the geometric ion-ion cross sections primarily due to Bound-Free Pair Production (BFPP) and Electro-Magnetic Dissociation (EMD). Apart from a general interest in verifying the calculations experimentally, an accurate prediction of the losses created in the heavy ion collisions is of practical interest for the LHC, where some collision products are lost in cryogenically cooled magnets and have the potential to quench these magnets. In the 2012 RHIC run uranium ions collided with each other at $sqrt{s_{NN}} = 192.8$ GeV with nearly all beam losses due to collisions. This allows for the measurement of the total cross section, which agrees with the calculated cross section within the experimental error.
To rectify the problems of electron clouds observed in RHIC and unacceptable ohmic heating for superconducting magnets that can limit future machine upgrades, we started developing a robotic plasma deposition technique for $in-situ$ coating of the RH IC 316LN stainless steel cold bore tubes based on staged magnetrons mounted on a mobile mole for deposition of Cu followed by amorphous carbon (a-C) coating. The Cu coating reduces wall resistivity, while a-C has low SEY that suppresses electron cloud formation. Recent RF resistivity computations indicate that 10 {mu}m of Cu coating thickness is needed. But, Cu coatings thicker than 2 {mu}m can have grain structures that might have lower SEY like gold black. A 15-cm Cu cathode magnetron was designed and fabricated, after which, 30 cm long samples of RHIC cold bore tubes were coated with various OFHC copper thicknesses; room temperature RF resistivity measured. Rectangular stainless steel and SS discs were Cu coated. SEY of rectangular samples were measured at room; and, SEY of a disc sample was measured at cryogenic temperatures.
We have studied the time evolution of the heavy ion luminosity and bunch intensities in the Relativistic Heavy Ion Collider (RHIC), at BNL, and in the Large Hadron Collider (LHC), at CERN. First, we present measurements from a large number of RHIC st ores (from Run 7), colliding 100 GeV/nucleon Au beams without stochastic cooling. These are compared with two different calculation methods. The first is a simulation based on multi-particle tracking taking into account collisions, intrabeam scattering, radiation damping, and synchrotron and betatron motion. In the second, faster, method, a system of ordinary differential equations with terms describing the corresponding effects on emittances and bunch populations is solved numerically. Results of the tracking method agree very well with the RHIC data. With the faster method, significant discrepancies are found since the losses of particles diffusing out of the RF bucket due to intrabeam scattering are not modeled accurately enough. Finally, we use both methods to make predictions of the time evolution of the future Pb beams in the LHC at injection and collision energy. For this machine, the two methods agree well.
mircosoft-partner

هل ترغب بارسال اشعارات عن اخر التحديثات في شمرا-اكاديميا