Reduction of interfacial thermal resistance of overlapped graphene by bonding carbon chains

81   0   0.0 ( 0 )
 Added by Huang Yuwen
 Publication date 2020
  fields Physics
and research's language is English




Ask ChatGPT about the research

Exploring the mechanism of interfacial thermal transport and reducing the interfacial thermal resistance is of great importance for thermal management and modulation. Herein, the interfacial thermal resistance between overlapped graphene nanoribbons is largely reduced by adding bonded carbon chains by performing molecular dynamics simulations. And the analytical model (cross-interface model, CIM) is utilized to analyze and explain the two-dimensional thermal transport mechanism at cross-interface. An order of magnitude reduction in interfacial thermal resistance is found as the graphene nanoribbons are bonded by just one carbon chain. Interestingly, the decreasing rate of interfacial thermal resistance slows down gradually with the increasing of the number of carbon chains, which can be explained by the proposed theoretical relationship based on CIM. Moreover, by the comparison of CIM and traditional simplified model, the accuracy of CIM is verified and demonstrated in overlapped graphene nanoribbons. This work provides a new way to improve the interfacial thermal transport and reveal the essential mechanism for low-dimensional materials applied in thermal management.



rate research

Read More

We proposed a new way, adding intertube atoms, to enhance interfacial thermal conductance (ITC) between SiC-carbon nanotube (CNT) array structure. Non-equilibrium molecular dynamics method was used to study the ITC. The results show that the intertube atoms can significantly enhance the ITC. The dependence of ITC on both the temperature and the number of intertube atoms are shown. The mechanism is analyzed by calculating probability distributions of atomic forces and vibrational density of states. Our study may provide some guidance on enhancing the ITC of CNT-based composites.
We present an atomic-resolution observation and analysis of graphene constrictions and ribbons with sub-nanometer width. Graphene membranes are studied by imaging side spherical aberration-corrected transmission electron microscopy at 80 kV. Holes are formed in the honeycomb-like structure due to radiation damage. As the holes grow and two holes approach each other, the hexagonal structure that lies between them narrows down. Transitions and deviations from the hexagonal structure in this graphene ribbon occur as its width shrinks below one nanometer. Some reconstructions, involving more pentagons and heptagons than hexagons, turn out to be surprisingly stable. Finally, single carbon atom chain bridges between graphene contacts are observed. The dynamics are observed in real time at atomic resolution with enough sensitivity to detect every carbon atom that remains stable for a sufficient amount of time. The carbon chains appear reproducibly and in various configurations from graphene bridges, between adsorbates, or at open edges and seem to represent one of the most stable configurations that a few-atomic carbon system accomodates in the presence of continuous energy input from the electron beam.
272 - Adili Aiyiti , Xue Bai , Jing Wu 2018
Establishment of a new technique or extension of an existing technique for thermal and thermoelectric measurements to a more challenging system is an important task to explore the thermal and thermoelectric properties of various materials and systems. The bottleneck lies in the challenges in measuring the thermal contact resistance. In this work, we applied electron beam self-heating technique to derive the intrinsic thermal conductivity of suspended Molybdenum Disulfide (MoS2) ribbons and the thermal contact resistance, with which the interfacial thermal resistance between few-layer MoS2 and Pt electrodes was calculated. The measured room temperature thermal conductivity of MoS2 is around 30 W/mK, while the estimated interfacial thermal resistance is around 2*10-6 m2K/W. Our experiments extend a useful branch in application of this technique for studying thermal properties of suspended layered ribbons and have potential application in investigating the interfacial thermal resistance of different 2D heterojunctions.
We report large-yield production of graphene flakes on glass by anodic bonding. Under optimum conditions, we counted several tens of flakes with lateral size around 20-30 {mu}m and few tens of flakes with larger size. 60-70% of the flakes have negligible D peak. We show that it is possible to easily transfer the flakes by wedging technique. The transfer on silicon does not damage graphene and lowers the doping. The charge mobility of the transferred flakes on silicon is of the order of 6000 cm^2/V s (at carrier concentration of 10^12 cm^-2), which is typical for devices prepared on this substrate with exfoliated graphene.
Capillary and van der Waals forces cause nanotubes to deform or even collapse under metal contacts. Using ab-initio bandstructure calculations, we find that these deformations reduce the bandgap by as much as 30%, while fully collapsed nanotubes become metallic. Moreover degeneracy lifting, due to the broken axial symmetry and wavefunctions mismatch between the fully collapsed and the round portions of a CNT, leads to a three times higher contact resistance. The latter we demonstrate by contact resistance calculations within the tight-binding approach.