Evolution of the metallic state of LaNiO$_3$/LaAlO$_3$ superlattices measured by $^8$Li $beta$-detected NMR


الملخص بالإنكليزية

Using ion-implanted $^8$Li $beta$-detected NMR, we study the evolution of the correlated metallic state of LaNiO$_3$ in a series of LaNiO$_3$/LaAlO$_3$ superlattices as a function of bilayer thickness. Spin-lattice relaxation measurements in an applied field of 6.55 T reveal two equal amplitude components: one with metallic ($T$-linear) $1/T_{1}$, and a second with a more complex $T$-dependence. The metallic character of the slow relaxing component is only weakly affected by the LaNiO$_3$ thickness, while the fast component is much more sensitive, exhibiting the opposite temperature dependence (increasing towards low $T$) in the thinnest, most magnetic samples. The origin of this bipartite relaxation is discussed.