In this research, specimens of aluminum alloy 6061 were received, and chemical composition was investigated. After that solution heat treatment was applied on it at 530°C, a section of these specimens was quenched in water and anther quenched in oil, and two sections were aged at 160°C for times (1,3,5 h), and thus obtained six samples differ in condition of heat treatment in addition to as received specimen.