The purpose of this study was to compare the shear bond strength to root dentin of a nano- ionomer material (Ketac N100,3M) and a fifth generation bonding material (Excite,Vivadent) applied with a resin composite (Tetric-ceram,Vivadent), in order to determine the material of choice for restoring root extended lesions.