In this work we shed light on the early stage of the chemical vapor deposition of graphene on Ge(001) surfaces. By a combined use of microRaman and x-ray photoelectron spectroscopies, and scanning tunneling microscopy and spectroscopy, we were able to individuate a carbon precursor phase to graphene nucleation which coexists with small graphene domains. This precursor phase is made of C aggregates with different size, shape and local ordering which are not fully sp2 hybridized. In some atomic size regions these aggregates show a linear arrangement of atoms as well as the first signature of the hexagonal structure of graphene. The carbon precursor phase evolves in graphene domains through an ordering process, associated to a re-arrangement of the Ge surface morphology. This surface structuring represents the embryo stage of the hills-and-valleys faceting featured by the Ge(001) surface for longer deposition times, when the graphene domains coalesce to form a single layer graphene film.



rate research

Read More

Germanium is emerging as the substrate of choice for the growth of graphene in CMOS-compatible processes. For future application in next generation devices the accurate control over the properties of high-quality graphene synthesized on Ge surfaces, such as number of layers and domain size, is of paramount importance. Here we investigate the role of the process gas flows on the CVD growth of graphene on Ge(100). The quality and morphology of the deposited material is assessed by using microRaman spectroscopy, x-ray photoemission spectroscopy, scanning electron and atomic force microscopies. We find that by simply varying the carbon precursor flow different growth regimes - yielding to graphene nanoribbons, graphene monolayer and graphene multilayer - are established. We identify the growth conditions yielding to a layer-by-layer growth regime and report on the achievement of homogeneous monolayer graphene with an average intensity ratio of 2D and G bands in the Raman map larger than 3.
175 - Zhuhua Zhang , , Wanlin Guo 2009
We show by first-principles calculations that the electronic properties of zigzag graphene nanoribbons (Z-GNRs) adsorbed on Si(001) substrate strongly depend on ribbon width and adsorption orientation. Only narrow Z-GNRs with even rows of zigzag chains across their width adsorbed perpendicularly to the Si dimer rows possess an energy gap, while wider Z-GNRs are metallic due to width-dependent interface hybridization. The Z-GNRs can be metastably adsorbed parallel to the Si dimer rows, but show uniform metallic nature independent of ribbon width due to adsorption induced dangling-bond states on the Si surface.
The practical difficulties to use graphene in microelectronics and optoelectronics is that the available methods to grow graphene are not easily integrated in the mainstream technologies. A growth method that could overcome at least some of these problems is chemical vapour deposition (CVD) of graphene directly on semiconducting (Si or Ge) substrates. Here we report on the comparison of the CVD and molecular beam epitaxy (MBE) growth of graphene on the technologically relevant Ge(001)/Si(001) substrate from ethene (C$_2$H$_4$) precursor and describe the physical properties of the films as well as we discuss the surface reaction and diffusion processes that may be responsible for the observed behavior. Using nano angle resolved photoemission (nanoARPES) complemented by transport studies and Raman spectroscopy, we report the direct observation of massless Dirac particles in monolayer graphene, providing a comprehensive mapping of their low-hole doped Dirac electron bands. The micrometric graphene flakes are oriented along two predominant directions rotated by $30^circ$ with respect to each other. The growth mode is attributed to the mechanism when small graphene molecules nucleate on the Ge(001) surface and it is found that hydrogen plays a significant role in this process.
We report on a systematic study of the growth of epitaxial TiO2 films deposited by pulsed laser deposition on Ti-terminated (001) SrTiO3 single crystals. By using in-situ reflection high energy electron diffraction, low energy electron diffraction, x-ray photoemission spectroscopy and scanning probe microscopy, we show that the stabilization of the anatase (001) phase is preceded by the growth of a pseudomorphic Sr-Ti-O intermediate layer, with a thickness between 2 and 4 nm. The data demonstrate that the formation of this phase is related to the activation of long range Sr migration from the substrate to the film. The role of interface Gibbs energy minimization, as a driving force for Sr diffusion, is discussed. Our results enrich the phase diagram of the Sr-Ti-O system under epitaxial strain opening the roudeficient SrTiO phase.
By combining scanning probe microscopy with Raman and x-ray photoelectron spectroscopies, we investigate the evolution of CVD-grown graphene/Ge(001) as a function of the deposition temperature in close proximity to the Ge melting point, highlighting an abrupt change of the graphenes quality, morphology, electronic properties and growth mode at 930 degrees. We attribute this discontinuity to the incomplete surface melting of the Ge substrate and show how incomplete melting explains a variety of diverse and long-debated peculiar features of the graphene/Ge(001), including the characteristic nanostructuring of the Ge substrate induced by graphene overgrowth. We find that the quasi-liquid Ge layer formed close to 930 degrees is fundamental to obtain high-quality graphene, while a temperature decrease of 10 degrees already results in a wrinkled and defective graphene film.
comments
Fetching comments Fetching comments
Sign in to be able to follow your search criteria
mircosoft-partner

هل ترغب بارسال اشعارات عن اخر التحديثات في شمرا-اكاديميا