No Arabic abstract
Detectors proposed for the International Linear Collider (ILC) incorporate a tungsten sampling calorimeter (`BeamCal) intended to reconstruct showers of electrons, positrons and photons that emerge from the interaction point of the collider with angles between 5 and 50 milliradians. For the innermost radius of this calorimeter, radiation doses at shower-max are expected to reach 100 MRad per year, primarily due to minimum-ionizing electrons and positrons that arise in the induced electromagnetic showers of e+e- `beamstrahlung pairs produced in the ILC beam-beam interaction. However, radiation damage to calorimeter sensors may be dominated by hadrons induced by nuclear interactions of shower photons, which are much more likely to contribute to the non-ionizing energy loss that has been observed to damage sensors exposed to hadronic radiation. We report here on the results of SLAC Experiment T-506, for which several different types of silicon diode sensors were exposed to doses of radiation induced by showering electrons of energy 3.5-10.6 GeV. By embedding the sensor under irradiation within a tungsten radiator, the exposure incorporated hadronic species that would potentially contribute to the degradation of a sensor mounted in a precision sampling calorimeter. Depending on sensor technology, efficient charge collection was observed for doses as large as 220 MRad.
The International Large Detector (ILD) is a proposed detector for the International Linear Collider (ILC). It has been designed to achieve an excellent jet energy resolution by using Particle Flow Algorithms (PFA), which rely on the ability to separate nearby particles within jets. PFA requires calorimeters with high granularity. The ILD Electromagnetic Calorimeter (ECAL) is a sampling calorimeter with thirty tungsten absorber layers. The total thickness of this ECAL is about 24 X$_0$, and it has between 10 and 100 million channels to make high granularity. Silicon sensors are a candidate technology for the sensitive layers of this ECAL. Present prototypes of these sensors have 256 5.5$times$5.5 mm$^2$ pixels in an area of 9$times$9 cm$^2$.We have measured various properties of these prototype sensors: the leakage current, capacitance, and full depletion voltage. We have also examined the response to an infrared laser to understand the sensors response at its edge and between pixel readout pads, as well the effect of different guard ring designs. In this paper, we show results from these measurements and discuss future works.
Two special calorimeters are foreseen for the instrumentation of the very forward region of the ILC detector, a luminometer designed to measure the rate of low angle Bhabha scattering events with a precision better than 10-3 and a low polar angle calorimeter, adjacent to the beam-pipe. The latter will be hit by a large amount of beamstrahlung remnants. The amount and shape of these depositions will allow a fast luminosity estimate and the determination of beam parameters. The sensors of this calorimeter must be radiation hard. Both devices will improve the hermeticity of the detector in the search for new particles. Finely segmented and very compact calorimeters will match the requirements. Due to the high occupancy fast front-end electronics is needed. The design of the calorimeters developed and optimised with Monte Carlo simulations is presented. Sensors and readout electronics ASICs have been designed and prototypes are available. Results on the performance of these major components are summarised.
The Mu2e calorimeter is composed of 1400 un-doped CsI crystals, coupled to large area UV extended Silicon Photomultipliers (SiPMs), arranged in two annular disks. This calorimeter has to provide precise information on energy, timing and position resolutions. It should also be fast enough to handle the high rate background and it must operate and survive in the high radiation environment. Simulation studies estimated that, in the highest irradiated regions, each photo-sensor will absorb a dose of 20 krad and will be exposed to a neutron fluency of 5.5x10^11 n_(1MeV)/cm^2 in three years of running, with a safety factor of 3 included. At the end of 2015, we have concluded an irradiation campaign at the Frascati Neutron Generator (FNG, Frascati, Italy) measuring the response of two different 16 array models from Hamamatsu, which differ for the protection windows and a SiPM from FBK. In 2016, we have carried out two additional irradiation campaigns with neutrons and photons at the Helmholtz-Zentrum Dresden-Rossendorf (HZDR, Dresden, Germany) and at the Calliope gamma irradiation facility at ENEA-Casaccia, respectively. A negligible increment of the leakage current and no gain change have been observed with the dose irradiation. On the other hand, at the end of the neutron irradiation, the gain does not show large changes whilst the leakage current increases by around a factor of 2000. In these conditions, the too high leakage current makes problematic to bias the SiPMs, thus requiring to cool them down to a running temperature of ~0 {deg}C.
We are developing position sensitive silicon detectors (PSDs) which have an electrode at each of four corners so that incident position of a charged particle can be obtained with signal from the electrodes. It is expected that the position resolution of the electromagnetic calorimeter (ECAL) of the ILD detector will be improved by introducing PSDs to detection layers. We have been developing the PSDs for several years. In the previous production we found that the charge separation is not optimally done due to the readout impedance. To solve the issue, we produced new PSDs with higher surface resistance with an additional resistive layer on the surface. We also implemented several techniques to decrease position distortion and increase signal-to-noise ratio which are essential for the optimal position resolution. The measurements on the prototype sensors are ongoing, including radiation source measurement and laser measurement using an ASIC for silicon pad detectors.
High-Voltage Monolithic Active Pixel Sensors (HV-MAPS) based on the 180 nm HV-CMOS process have been proposed to realize thin, fast and highly integrated pixel sensors. The MuPix7 prototype, fabricated in the commercial AMS H18 process, features a fully integrated on-chip readout, i.e. hit-digitization, zero suppression and data serialization. It is the first fully monolithic HV-CMOS pixel sensor that has been tested for the use in high irradiation environments like HL-LHC. We present results from laboratory and test beam measurements of MuPix7 prototypes irradiated with neutrons (up to $5.0cdot10^{15}{,rm{n}_{rm{eq}}/cm^2}$) and protons (up to $7.8cdot 10^{15} ,rm{protons}/cm^2$) and compare the performance with non-irradiated sensors. Efficiencies well above 90 % at noise rates below 200 Hz per pixel are measured. A time resolution better than 22 ns is measured for all tested settings and sensors, even at the highest irradiation fluences. The data transmission at 1.25 Gbit/s and the on-chip PLL remain fully functional.