Future experiments will use silicon sensors in the harsh radiation environment of the LHC (Large Hadron Collider) and high magnetic fields. The drift direction of the charge carriers is affected by the Lorentz force due to the high magnetic field. Also the resulting radiation damage changes the properties of the drift. In this paper measurements of the Lorentz angle of electrons and holes before and after irradiation are reviewed and compared with a simple algorithm to compute the Lorentz angle.
Future experiments are using silicon detectors in a high radiation environment and in high magnetic fields. The radiation tolerance of silicon improves by cooling it to temperatures below 180 K. At low temperatures the mobility increases, which leads
to larger deflections of the charge carriers by the Lorentz force. A good knowledge of the Lorentz angle is needed for design and operation of silicon detectors. We present measurements of the Lorentz angle between 77 K and 300 K before and after irradiation with a primary beam of 21 MeV protons.
This paper describes the performance of a prototype timing detector, based on 50 micrometer thick Ultra Fast Silicon Detector, as measured in a beam test using a 180 GeV/c momentum pion beam. The dependence of the time precision on the pixel capacita
nce and the bias voltage is investigated here. A timing precision from 30 ps to 100 ps, depending on the pixel capacitance, has been measured at a bias voltage of 180 V. Timing precision has also been measured as a function of the bias voltage.
While the tracking detectors of the ATLAS and CMS experiments have shown excellent performance in Run 1 of LHC data taking, and are expected to continue to do so during LHC operation at design luminosity, both experiments will have to exchange their
tracking systems when the LHC is upgraded to the high-luminosity LHC (HL-LHC) around the year 2024. The new tracking systems need to operate in an environment in which both the hit densities and the radiation damage will be about an order of magnitude higher than today. In addition, the new trackers need to contribute to the first level trigger in order to maintain a high data-taking efficiency for the interesting processes. Novel detector technologies have to be developed to meet these very challenging goals. The German groups active in the upgrades of the ATLAS and CMS tracking systems have formed a collaborative Project on Enabling Technologies for Silicon Microstrip Tracking Detectors at the HL-LHC (PETTL), which was supported by the Helmholtz Alliance Physics at the Terascale during the years 2013 and 2014. The aim of the project was to share experience and to work together on key areas of mutual interest during the R&D phase of these upgrades. The project concentrated on five areas, namely exchange of experience, radiation hardness of silicon sensors, low mass system design, automated precision assembly procedures, and irradiations. This report summarizes the main achievements.
A detailed study of charge collection efficiency has been performed on the Silicon Drift Detectors (SDD) of the ALICE experiment. Three different methods to study the collected charge as a function of the drift time have been implemented. The first a
pproach consists in measuring the charge at different injection distances moving an infrared laser by means of micrometric step motors. The second method is based on the measurement of the charge injected by the laser at fixed drift distance and varying the drift field, thus changing the drift time. In the last method, the measurement of the charge deposited by atmospheric muons is used to study the charge collection efficiency as a function of the drift time. The three methods gave consistent results and indicated that no charge loss during the drift is observed for the sensor types used in 99% of the SDD modules mounted on the ALICE Inner Tracking System. The atmospheric muons have also been used to test the effect of the zero-suppression applied to reduce the data size by erasing the counts in cells not passing the thresholds for noise removal. As expected, the zero suppression introduces a dependence of the reconstructed charge as a function of drift time because it cuts the signal in the tails of the electron clouds enlarged by diffusion effects. These measurements allowed also to validate the correction for this effect extracted from detailed Monte Carlo simulations of the detector response and applied in the offline data reconstruction.
The development of Low-Gain Avalanche Detectors has opened up the possibility of manufacturing silicon detectors with signal larger than that of traditional sensors. In this paper we explore the timing performance of Low-Gain Avalanche Detectors, and
in particular we demonstrate the possibility of obtaining ultra-fast silicon detector with time resolution of less than 20 picosecond.