ﻻ يوجد ملخص باللغة العربية
The question of the correlation between magnetization, band splittings, and magnetic circular dichroism (MCD) in the fundamental gap region of dilute magnetic semiconductors is examined experimentally and theoretically taking the case of wurtzite Ga(1-x)FexN as an example. Magnetization and polarization-resolved reflectivity measurements have been performed down to 2K and up to 7T for x = 0.2%. Optical transitions originating from all three free excitons A, B and C, specific to the wurtzite structure, have been observed and their evolution with the magnetic field determined. It is demonstrated that the magnitude of the exciton splittings evaluated from reflectivity-MCD data can be overestimated by more than a factor of 2, as compared to the values obtained by describing the polarization-resolved reflectivity spectra with appropriate dielectric functions. A series of model calculations shows that the quantitative inaccuracy of MCD originates from a substantial influence of the magnetization-dependent exchange interactions not only on the spin splittings of excitons but also upon their linewidth and oscillator strength. At the same time, a method is proposed that allows to evaluate the field and temperature dependencies of the magnetization from MCD spectra. The accurate values of the excitonic splittings and of the magnetization reported here substantiate the magnitudes of the apparent $sp-d$ exchange integrals in (Ga,Fe)N previously determined.
We report on the metalorganic chemical vapor deposition (MOCVD) of GaN:Fe and (Ga,Fe)N layers on c-sapphire substrates and their thorough characterization via high-resolution x-ray diffraction (HRXRD), transmission electron microscopy (TEM), spatiall
Fe-doped III-V ferromagnetic semiconductors (FMSs) such as (In,Fe)As, (Ga,Fe)Sb, (In,Fe)Sb, and (Al,Fe)Sb are promising materials for spintronic device applications because of the availability of both n- and p-type materials and the high Curie temper
A systematic investigation about the structure and magnetism of Fe75-xCr25Gax (11<x<33) and Fe50Cr50-yGay (0<y<33) series has been carried out in this work. It shows that the parent Fe50Cr25Ga25 phase has higher tolerance for Ga replacing Cr than rep
The magnetic properties of as-grown Ga$_{1-x}$Mn$_{x}$As have been investigated by the systematic measurements of temperature and magnetic field dependent soft x-ray magnetic circular dichroism (XMCD). The {it intrinsic} XMCD intensity at high temper
The difference in the transmission for left and right circularly polarised light though thin films on substrates in a magnetic field is used to obtain the magnetic circular dichroism of the film. However there are reflections at all the interfaces an